The Measurement of Original Residual Stress in Aircraft Aluminum Alloy
-
摘要: 为提高裂纹柔度法测试铝合金预拉伸板材毛坯初始残余应力的测试效率和测试精度,从应变采集精度和柔度函数计算效率等方面展开研究,采用基于ABAQUS有限元软件Load Case功能对柔度函数的算法进行了优化。对铝合金预拉伸板7050-T7451的毛坯初始残余应力进行了测试,建立了裂纹柔度法残余应力高效、高精度测量的测试规程,给出了突发状况应对机制。结果表明:柔度函数的计算效率得到显著提升,获得了该板材轧制方向和横向方向的残余应力均呈明显"M型曲线"的分布规律。Abstract: In order to improve the measuring accuracy and efficiency,the crack compliance method was adopted to measure the original residual stresses in the pre-stretched aluminum alloy plates,the accuracy of the measured strain and the computational efficiency of the compliance functions were discussed. The "Load Case"of ABAQUS software was applied to optimize the calculation method of compliance function. Then,the original residual stresses in the pre-stretched aluminum alloy plate 7050-T7451 were measured. The high efficiency,high precision measurement procedures of residual stress and emergency response mechanism were established based on the crack compliance method. The calculated results show the computational efficiency was improved obviously; "M type curves"of residual stresses were obtained for the rolling and the transverse directions.
-
Key words:
- ABAQUS /
- aircraft /
- aluminum alloys /
- crack compliance method /
- FORTRAN (programming language)
-
[1] 王树宏,马康民,马骏. 预拉伸铝合金板 7075T7351 内部残余应力分布测试[J]. 空军工程大学学报,2004,5(3):19-21Wang S H,Ma K M,Ma J. Method of measuring theresidual stress distribution in pre-stretched aluminumalloy plate 7075T7351 [J]. Journal of Air ForceEngineering University,2004,5(3):19-21 (in Chinese) [2] 王秋成,柯映林,章巧芳. 7075 铝合金板材残余应力深度梯度的评估[J]. 航空学报,2003,24(4):336-338Wang Q C,Ke Y L,Zhang Q F. Evaluation of residualstress depth profiling in 7075 aluminum alloy plates[J].Acta Aeronautica Et Astronautica Sinica,2003,24(4):336-338 (in Chinese) [3] Prime M B,Hill M R. Residual stress,stress relief,andinhomogeneity in aluminum plate[J]. Scripta Materialia,2002,46(1):77-82 [4] 张旦闻,刘宏昭,刘平. 裂纹柔度法在7075 铝合金板残余应力检测中的应用[J]. 材料热处理学报,2006,27(2):127-131Zhang D W,Liu H Z,Liu P. Evaluation of residualstresses in 7075 aluminum alloy plate using crackcompliance method[J]. Transactions of Materials andHeat Treatment,2006,27(2):127-131 (in Chinese) [5] 唐志涛,刘战强,艾兴. 基于裂纹柔度法的铝合金预拉伸板内部残余应力测试[J]. 中国有色金属学报,2007,17(9):1405-1409Tang Z T,Liu Z Q,Ai X. Measuring residua stresses depthprofile in pre-stretched aluminum alloy plate using crackcompliance method[J]. The Chinese Journal of NonferrousMetals,2007,17(9):1404-1409 (in Chinese) [6] 柯映林,董辉跃. 7075 铝合金厚扳预拉伸模拟分析及其在淬火残余应力消除中的应用[J]. 中国有色金属学报,2004,14(4):639-645Ke Y L,Dong H Y. Pre-stretching process and itsapplication in reducing residual stress of quenched 7075aluminum alloy thick-plates[J]. The Chinese Journal ofNonferrous Metals,2004,14(4):639-645 (in Chinese) [7] 唐志涛,刘战强,艾兴. 裂纹柔度法中插值函数及其阶数选择研究 [J]. 武汉理工大学学报,2007,29(8):75-77Tang Z T,Liu Z Q,Ai X. Measuring residual stresses depthprofile in pre-stretched aluminum alloy plate using crackcompliance method[J]. The Chinese Journal of NonferrousMetals,2007,29(8):1404-1409 (in Chinese) [8] Prime M B. Experimental procedure for crack compliance(slitting) measurements of residual stress[R]. LosAlamos; Los Alamos National Laboratory Report,2003,LA-UR-03-8629 [9] Prime M B,Hill M R. Uncertainty analysis,model error,and order selection for series-expanded,residual stressinverse solution[J]. Journal of Engineering Materials andTechnology,2006,128(2):175-185
点击查看大图
计量
- 文章访问数: 164
- HTML全文浏览量: 38
- PDF下载量: 5
- 被引次数: 0