Articles:2022,Vol:27,Issue(3):158-176
Citation:
WEI Chen, JING Jianlong, DING Chen, QIAN Dongdong, GUO Yalin. Analysis of Fracture of Pre-sintered Zirconia Material in Neck Milling[J]. International Journal of Plant Engineering and Management, 2022, 27(3): 158-176

Analysis of Fracture of Pre-sintered Zirconia Material in Neck Milling
WEI Chen, JING Jianlong, DING Chen, QIAN Dongdong, GUO Yalin
Department of Prosthodontics, Stomatological Hospital of Nanjing University, Nanjing 210093, China
Abstract:
With the continuous improvement of the accuracy requirements of clinical base or base tooth and denture, the design of denture neck edge is becoming thinner and thinner, and the presintering zirconia dioxide billet for denture making evacuation and low strength material mechanical characteristics make the certain probability of denture neck edge fragmentation and peeling in the cutting process. Based on this phenomenon, the abnormal wear is the main reason, and a method of high frequency ultrasonic time cleaning to reduce the fracture of the denture neck in actual cutting is proposed.
Key words:    zirconium dioxide cutting    neck edge    fracture tool abnormal wear    high frequency cleaning   
Received: 2022-04-16     Revised:
DOI: 10.13434/j.cnki.1007-4546.2022.03003
Corresponding author:     Email:
Author description:
Service
PDF(4840KB) Free
Print
Authors
WEI Chen
JING Jianlong
DING Chen
QIAN Dongdong
GUO Yalin

References:
[1] ZHANG K. Clinical application and development trend of zirconia all-ceramic system in prosthodontics[J]. Electronic Journal of General Stomatology, 2015,2(12):8-9 (in Chinese)
[2] MA Q, SHI L Y, HUANG S X, et al. Research status and prospect of zirconia ceramics in the field of dental restoration[J]. China Tissue Engineering Research, 2021,25(22):3597-3602 (in Chinese)
[3] WANG C Y. Application effect of zirconia all-ceramic restoration in oral restoration[J]. Journal of Clinical Rational Drug Use, 2020,13(35):166-167 (in Chinese)
[4] OSAMA IBRAHIM E S, O'CONNELL A C. Successful restoration of severely mutilated primary incisors using a novel method to retain zirconia crowns-two year results[J]. The Journal of Clinical Pediatric Dentistry, 2016,40(6):425-430
[5] XUE J X. Basic research on high-speed milling of zirconia ceramics[D]. Nanjing University of Aeronautics and Astronautics, 2016 (in Chinese)
[6] LEI X B, XIE F, LIAO W H, et al. Experimental study on edge chipping of dental zirconia ceramics after milling[J]. Journal of Artificial Crystals, 2015,44(6):1662-1667+1674 (in Chinese)
[7] BIAN R. Basic research on precision milling of zirconia ceramics with diamond micro-milling cutter[D]. Nanjing University of Aeronautics and Astronautics, 2014 (in Chinese)
[8] BIAN R, HE N, LI L, et al. Analysis of milling force characteristics in micro-milling zirconia ceramics[J]. China Mechanical Engineering, 2014,25(23):3200-3206 (in Chinese)
[9] LEI X B. Research on key technology and equipment of high speed milling of pre-sintered zirconia denture[D]. Nanjing University of Aeronautics and Astronautics, 2012 (in Chinese)
[10] MA L L, ZUO Y C, WANG X, et al. Wear mechanism and theoretical model of zirconia ceramic turning tools[J]. Journal of Northeastern University (Natural Science Edition), 2020,41(7):955-961 (in Chinese)
[11] WU H B, ZUO D W, SUN Q P, et al. Tool wear in milling of zirconia bioceramics[J]. China Mechanical Engineering, 2015,26(7):960-964+993
[12] DING Z. Study on machining performance of powder metallurgy materials in high speed machining[]. Hefei University of Technology, 2016 (in Chinese)
[13] LI Z. Analysis on the causes and countermeasures of mechanical vibration in machining process[J]. Internal Combustion Engines and Accessories, 2019(11):256-257 (in Chinese)
[14] LI Y L. Principle and practical application of ultrasonic cleaning[J]. Purge the World, 2006(7):31-35 (in Chinese)