泡沫镍夹层结构自冲铆接头的成形特征及失效机理分析

丁文有 何晓聪 刘佳沐 曾凯

丁文有, 何晓聪, 刘佳沐, 曾凯. 泡沫镍夹层结构自冲铆接头的成形特征及失效机理分析[J]. 机械科学与技术, 2018, 37(4): 581-585. doi: 10.13433/j.cnki.1003-8728.2018.0414
引用本文: 丁文有, 何晓聪, 刘佳沐, 曾凯. 泡沫镍夹层结构自冲铆接头的成形特征及失效机理分析[J]. 机械科学与技术, 2018, 37(4): 581-585. doi: 10.13433/j.cnki.1003-8728.2018.0414
Ding Wenyou, He Xiaocong, Liu Jiamu, Zeng Kai. Forming Characteristics and Failure Mechanism Analysis of Sandwich Structure Self-piercing Riveted Joint with Nickel Foam[J]. Mechanical Science and Technology for Aerospace Engineering, 2018, 37(4): 581-585. doi: 10.13433/j.cnki.1003-8728.2018.0414
Citation: Ding Wenyou, He Xiaocong, Liu Jiamu, Zeng Kai. Forming Characteristics and Failure Mechanism Analysis of Sandwich Structure Self-piercing Riveted Joint with Nickel Foam[J]. Mechanical Science and Technology for Aerospace Engineering, 2018, 37(4): 581-585. doi: 10.13433/j.cnki.1003-8728.2018.0414

泡沫镍夹层结构自冲铆接头的成形特征及失效机理分析

doi: 10.13433/j.cnki.1003-8728.2018.0414
基金项目: 

国家自然科学基金项目(51565023,51565022)资助

详细信息
    作者简介:

    丁文有(1993-),硕士研究生,研究方向为薄板材料连接新技术,daland121834@163.com

    通讯作者:

    何晓聪,教授,博士生导师.xiaocong_he@126.com

Forming Characteristics and Failure Mechanism Analysis of Sandwich Structure Self-piercing Riveted Joint with Nickel Foam

  • 摘要: 为揭示泡沫镍夹层结构自冲铆接头的成形特征及失效机理,本文制备了以AA5052铝合金为基板,泡沫镍为夹层的自冲铆接头;采用理论分析与微观组织观察相结合的方法对夹层结构接头成形特征进行系统研究,通过拉伸-剪切试验研究接头的静失效载荷及失效位移,探究了接头的失效机理。结果表明:泡沫镍夹层可增大接头的钉脚张开度,并改善应力分布;铆接过程中泡沫镍能在铆接界面间形成牢固的自润滑物理吸附膜,可提高接头的耐腐蚀性;1mm泡沫镍夹层使接头静失效载荷增加了8.9%;随着泡沫镍夹层厚度的增加,接头的抗拉强度呈降低趋势;泡沫镍夹层结构自冲铆接头的失效模式为铆钉脱离下板,上板主要承受拉伸载荷,下板承受压缩载荷。
  • [1] Li D Z, Han L, Chrysanthou A, et al. The effect of setting velocity on the static and fatigue strengths of self-piercing riveted joints for automotive applications[C]//Proceedings of the 143rd Annual Meeting & Exhibition. Cham:Springer, 2014
    [2] Zhang X L, He X C, Xing B Y, et al. Influence of heat treatment on fatigue performances for self-piercing riveting similar and dissimilar titanium, aluminium and copper alloys[J]. Materials & Design, 2016,97:108-117
    [3] He X C, Zhao L, Deng C J, et al. Self-piercing riveting of similar and dissimilar metal sheets of aluminum alloy and copper alloy[J]. Materials & Design, 2015,65:923-933
    [4] Yan W M, Xie Z Q, Yu C, et al. Experimental investigation and design method for the shear strength of self-piercing rivet connections in thin-walled steel structures[J]. Journal of Constructional Steel Research, 2017,133:231-240
    [5] Li D Z. Influence of aluminium sheet surface modification on the self-piercing riveting process and the joint static lap shear strength[J]. The International Journal of Advanced Manufacturing Technology, 2017,93(5-8):2685-2695
    [6] Hirsch F, M?ller S, Machens M, et al. Simulation of self-piercing rivetting processes in fibre reinforced polymers:material modelling and parameter identification[J]. Journal of Materials Processing Technology, 2017,241:164-177
    [7] 张羽,朱颖,郭伟,等.含泡沫镍中间层陶瓷/不锈钢接头微观组织和性能[J].北京航空航天大学学报,2016,42(11):2488-2494 Zhang Y, Zhu Y, Guo W, et al. Microstructure and properties of ceramic/stainless steel joint with Ni foam interlayer[J]. Journal of Beijing University of Aeronautics and Astronautics, 2016,42(11):2488-2494(in Chinese)
    [8] Han L, Chrysanthou A, Young K W. Mechanical behaviour of self-piercing riveted multi-layer joints under different specimen configurations[J]. Materials & Design, 2007,28(7):2024-2033
    [9] Gay A, Lefebvre F, Bergamo S, et al. Fatigue of aluminum/glass fiber reinforced polymer composite assembly joined by self-piercing riveting[J]. Procedia Engineering, 2015,133:501-507
    [10] Fan S F, Zhang T, Yu K, et al. Compressive properties and energy absorption characteristics of open-cell nickel foams[J]. Transactions of Nonferrous Metals Society of China, 2017,27(1):117-124
    [11] 张景怀,惠志林,方政秋.泡沫镍的制备工艺与性能[J].稀有金属,2001,25(3):230-234 Zhang J H, Hui Z L, Fang Z Q. Preparation and performance of nickel foam[J]. Chinese Journal of Rare Metals, 2001,25(3):230-234(in Chinese)
    [12] 李宇,沈伟,赵鹏,等.泡沫铜压缩屈服强度有限元计算方法[J].粉末冶金技术,2017,35(1):3-9 Li Y, Shen W, Zhao P, et al. Finite element analysis for the yield strength of copper foam[J]. Powder Metallurgy Technology, 2017,35(1):3-9(in Chinese)
    [13] 黄东梅.闭孔泡沫材料几何建模及其应用研究[D].秦皇岛:燕山大学,2014 Huang D M. Research on geometry modeling for closed cell foam material and its application[D]. Qinhuangdao:Yanshan University, 2014(in Chinese)
    [14] 徐丹,王中禹.计量测试中异常数据剔除的措施[J].科技经济导刊,2016,(20):62 Xu D, Wang Z Y. Eliminate the abnormal data in the measurement of measures of[J]. Technology and Economic Guide, 2016,(20):62(in Chinese)
    [15] Haque R, Durandet Y. Strength prediction of self-pierce riveted joint in cross-tension and lap-shear[J]. Materials & Design, 2016,108:666-678
  • 加载中
计量
  • 文章访问数:  177
  • HTML全文浏览量:  37
  • PDF下载量:  9
  • 被引次数: 0
出版历程
  • 收稿日期:  2017-09-28
  • 刊出日期:  2018-04-05

目录

    /

    返回文章
    返回